Choosing the right BOPP film grade comes down to four variables: what the pack must do (seal, barrier, print, protect), the thickness your line can run, whether the film needs a heat-seal layer, and the surface finish the brand wants. This table compares every BOPP grade we manufacture against those four variables, so you can shortlist before requesting samples.
Last updated: 2026-11-28 · All values are typical figures from production test reports, tested at 23 °C / 50 % RH.
Quick comparison: all BOPP grades
| Grade | Thickness | Heat seal | Corona side | Haze | Typical use | Key property |
|---|---|---|---|---|---|---|
| BOPP Plain | 10–52 µm | No | 1 or 2 sides | ≤ 1.5 % | Printing, lamination, tape base, bag film | Highest clarity, best print base |
| BOPP Heat Sealable | 15–52 µm | 1 or 2 sides | 1 or 2 sides | ≤ 2.5 % | Snack bags, food pouches, overwrap | Sealable without adhesive |
| BOPP Pearlized | 18–40 µm | Both sides | 1 side | 75 %+ opacity | Ice cream, confectionery, soap | Opaque white, pearl lustre, low density |
| BOPP Metallized | 20–30 µm (up to 75) | No | 1 side | — | Snack, coffee, biscuit, barrier lamination | High moisture & light barrier |
| BOPP Matt | 12–18 µm | No | 1 or 2 sides | High | Premium print, matte lamination | Low-gloss, soft-touch finish |
| BOPP Thermal Lamination | 20–37 µm | EVA hot-melt layer | 1 side | < 5 % | Paper lamination, book covers, packaging | Bonds to print with heat only |
| BOPP Tape Base | 23–28 µm | No | 1 side | ≤ 2 % | Adhesive tape production | Controlled COF for coating lines |
| BOPP Anti-Fog | 20–45 µm | Yes | 1 or 2 sides | Low | Fresh produce, meat, frozen food | Stops condensation clouding |
| BOPP Cigarette | 20–25 µm | Yes | As specified | Low | Cigarette box wrap, bundle wrap | High gloss, tight shrink, low COF |
| BOPP Flower Wrap | 8–50 µm | As specified | 1 side | Very low | Bouquet, floral sleeve, gift | High transparency, colour range |
How to read this table
1. Thickness drives cost, stiffness and barrier
Thinner film costs less per square metre but gives less stiffness and barrier. The practical floors:
- 8–12 µm — floral wrap, very light lamination. Below 10 µm the film gets hard to run on standard converting lines.
- 15–18 µm — general printing and lamination. The most common starting point for new projects.
- 20–30 µm — food packaging, metallized base, tape base. Where most volume sits.
- 35–52 µm — bag film, heavy-duty wrap, applications needing stiffness.
2. Heat seal layer decides whether you need adhesive
If your pack is formed on a vertical or horizontal form-fill-seal machine, you almost certainly need a heat-sealable grade. Plain BOPP has no seal layer — it must be laminated to a sealable web (usually PE or CPP) before it can close a bag.
Two-side heat sealable film lets you seal film-to-film without a separate sealant web. That removes one lamination step, at a higher film cost.
3. Corona treatment decides printability
Corona treatment raises surface tension so ink and adhesive bond. Our standard is ≥ 38 mN/m, which suits solvent-based, water-based and UV inks.
- One side treated — normal for printing on one face only.
- Two sides treated — needed when printing both faces, or when laminating on one side and printing the other.
Untreated BOPP will not hold ink reliably. If a supplier cannot state surface tension, ask for it.
4. Opacity and finish decide shelf appearance
- Clear (haze ≤ 1.5 %) — shows the product. Best for retail where product visibility sells.
- Pearlized (75 %+ opacity) — hides the product, gives a premium white/pearl look. Density is lower than clear BOPP (0.55–0.75 g/cm³ vs ~0.91), so you get more square metres per kilogram.
- Metallized — mirror finish plus light and moisture barrier. Common for coffee, snacks, and anything light-sensitive.
- Matt — low gloss, soft-touch. Used where glare is a problem or the brand wants a premium uncoated look.
Selection by application
| If you are packing… | Start with | Thickness | Why |
|---|---|---|---|
| Snack / biscuit / confectionery | BOPP Metallized or Pearlized | 20–30 µm | Barrier + shelf appeal |
| Fresh produce, meat, frozen | BOPP Anti-Fog, heat sealable | 20–45 µm | Stops condensation clouding |
| Ice cream / tubs | BOPP Pearlized | 30–40 µm | Opaque, cold-resistant, printable |
| Cigarette boxes | BOPP Cigarette | 20–25 µm | Tight shrink, high gloss |
| Book covers, menus, cards | BOPP Thermal Lamination | 20–27 µm | Bonds to print with heat |
| Adhesive tape | BOPP Tape Base | 23–28 µm | Controlled COF, consistent width |
| Bouquets, gift wrap | BOPP Flower Wrap | 8–25 µm | Maximum transparency |
| General print / laminate | BOPP Plain | 15–18 µm | Cheapest printable base |
Technical specifications (test report values)
| Parameter | Unit | BOPP Plain | BOPP Heat Seal | BOPP Pearlized | Standard |
|---|---|---|---|---|---|
| Thickness | µm | 3–75 | 15–40 | 20–50 | GB/T 13950 |
| Tensile strength MD | MPa | ≥ 120 | ≥ 120 | ≥ 100 | GB/T 1040 |
| Tensile strength TD | MPa | ≥ 200 | ≥ 200 | ≥ 180 | GB/T 1040 |
| Elongation at break MD | % | 50–200 | 50–180 | ≤ 180 | GB/T 1040 |
| Haze | % | ≤ 1.5 | ≤ 2.5 | — | GB/T 2410 |
| Gloss (45°) | GU | ≥ 85 | ≥ 80 | 60–110 | GB/T 8807 |
| Surface tension | mN/m | ≥ 38 | ≥ 38 | ≥ 38 | GB/T 14216 |
| Heat seal strength | N/15mm | — | ≥ 3 | ≥ 3 | 120 °C, 0.3 MPa, 1 s |
| MVTR | g/m²·24h | — | ≤ 4 | — | 38 °C, 90 % RH |
| Density | g/cm³ | ~0.91 | ~0.91 | 0.55–0.75 | — |
| Width range | mm | 250–10,000 | 90–1,600 | 250–2,200 | Custom |
| Core diameter | inch | 1" / 2" / 3" / 6" | 1" / 2" / 3" / 6" | 3" / 6" | Standard |
MD = machine direction, TD = transverse direction. Values are typical, not guaranteed minima — request a batch-specific test report for incoming QC.
Common specification mistakes
Specifying thickness without tolerance. A 20 µm film at ±3 % is 19.4–20.6 µm. If your line is set for exactly 20 µm, that tolerance matters. State it.
Assuming all "heat sealable" BOPP seals the same. Seal initiation temperature ranges 100–140 °C depending on grade. A film that seals at 140 °C will not run on a line set to 110 °C.
Forgetting the treated side. If you print one side and laminate the other, you need to know which side is treated. Two-side treated film costs more but removes the risk of running the wrong face.
Mixing pearlized and clear in the same cost calculation. Pearlized BOPP is significantly less dense, so a kilogram covers more area. Compare on cost per 1,000 m², not cost per kilogram.
Over-specifying barrier. Metallized BOPP gives a good moisture barrier but is not a high-barrier structure on its own. For oxygen-critical packs (coffee, nuts), metallized BOPP is usually laminated to a sealant and sometimes combined with an EVOH or foil layer.
Frequently asked questions
What is the difference between BOPP and BOPET? BOPP is polypropylene — cheaper, better moisture barrier, heat-sealable in some grades, but lower temperature resistance (softens around 100 °C+). BOPET is polyester — stronger, higher temperature resistance (up to 150 °C+), better dimensional stability, but not heat-sealable on its own and roughly 2–3× the cost. Use BOPP for the print/web layer of a pack and BOPET where strength, heat resistance or electrical insulation matter.
What thickness BOPP should I use for a snack bag? Most snack bag structures use 20–30 µm metallized or pearlized BOPP as the print web, laminated to a 30–50 µm sealant (PE or CPP). The BOPP carries the print and barrier; the sealant carries the seal.
Can BOPP be heat sealed to itself? Only heat-sealable grades, and only seal-face to seal-face. Plain BOPP cannot be sealed to itself without an adhesive or a coated seal layer.
What is the minimum order quantity? Typical MOQ is one 20-foot container per grade and thickness, though we consolidate multiple thicknesses into a single container for trial orders. Ask for the current minimum on your specific grade.
Do you supply food-contact compliant BOPP? Yes — BOPP grades for direct food contact are produced to meet FDA and EU 10/2011 requirements. Request the compliance declaration with your order; it is issued per grade.
What is the HS code for BOPP film? BOPP film is classified under 3920.20 (plates, sheets, film of polymers of propylene). Our BOPP grades ship under 3920201000. BOPET film falls under 3920.62 and ships under 3920629000. See the export guide for the full breakdown.
Request samples or a data sheet
Tell us the application, thickness, width and estimated annual volume, and we will confirm the grade and send a batch-specific test report.
- Email: sale@boppfilmsale.com
- Phone / WhatsApp: +86 189 1965 9471
- Technical data sheets: Film specifications
- Full product range: Products
*Asia Pacific Industry Group Co., Limited (APIG / AEC GROUP) — packaging film manufacturer and exporter, Hefei, Anhui, China.*